Product Description: UL 04533EH2 is a copolymer of ethylene and vinyl acetate. Availability: Africa & Middle East, Asia Pacific and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
- Free Flowing Agent: Yes
Applications: - Compounding
- Hot Melt Adhesives
- Wire and Cable Compounds
Information provided by ExxonMobil |