MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Esenttia 06C30DA Impact Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Characteristics: Control reologhy Impact block copolymer polypropylene; excellent impact/stiffness balance; consistent processability lot to lot; high process speed and easy removal of the molded pieces; good superficial gloss; moderately narrow molecular weight distribution; with mold release and antistatic additive.

Recommended for: Extrusion compression molding or injection molding processes of closures for carbonated beverages or not, where high stiffness and impact resistance is necessary (warm or cold environmental); housewares; injection molding general purpose applications.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238B
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.34 MPa50 mm/min; ASTM D638
Elongation at Yield 6.3 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1516.8 MPa1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 106.76 J/mASTM D256-A
Gardner Impact 28.25 JASTM D5420A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer
Ineos B4020N1331 Polyethylene Copolymer
Esenttia 08H85-1 Homopolymer Polypropylene
NOVA Chemicals SCLAIR® 2710CC HDPE Injection Molding Resin
Ineos B4020N1332 Polyethylene Copolymer

PESEN045 / 184617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.