MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Aktiplast® M Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Processing promoter reducing viscosity and dispersing fillers, especially for compounds based on natural rubber and blends of natural rubber

Use: Aktiplast M has a viscosity reducing effect in natural and isoprene rubber and their compounds. In a temperature range from 60-150 °C, the reduction of viscosity is obtained by a combination of specially selected fatty acids in zinc salts with a metal complex as activator. The natural chain length distribution of rubber, such as it is shown in a mole weight distribution curve, is largely maintained. Only the part of the rubber with a higher molecular weight is reduced. The mastication effect of Aktiplast M is stopped by the addition of carbon black or fillers. A special advantage of Aktiplast M is the saving of one mixing step, as there is no storage time of the masticated rubber required. As a result of the improved solubility of the fatty acid zinc salts in the rubber Aktiplast M has a favorable effect on the filler dispersion. The incorporation of the fillers is accelerated. Mixing energy is reduced, and mixing time can be saved.

Application: Processing promoter reducing viscosity and dispersing fillers. For tires, rubber-to-metal bonding, primarily for compounds based on natural rubber and rubber blends

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Ash 12 - 14 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 95.0 - 110 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceBrown Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8251 / 208644

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.