MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quaker Quintolubric® 702-46 RD Water Glycol Hydraulic Fluid
Categories: Fluid

Material Notes:
  • Superior liquid and vapor phase corrosion protection
  • High viscosity index
  • Excellent shear stability
  • Excellent chemcial thermal and hydrolytic stability
Applications: QUINTOLUBRIC® 702-46 RD is a premium water-glycol fire resistant fluid formulated to for hydraulic equipment. It is designed to provide optimum performance in hydraulic systems where fire resistant fluids are required. QUINTOLUBRIC® 702-46 RD contains an adequate amount of water to prevent ignition that could occur in hydraulic systems operating under high pressure through sudden line ruptures or fluid contact with a high temperature source. This fluid includes additives that provide lubricity, corrosion protection, and the overall performance demanded by high performance hydraulic systems. QUINTOLUBRIC® 702-46 RD provides a high viscosity index, low pour point, and excellent heat transfer and antifoam performance. These properties, along with the addition of an antiwear component, provide extended pump life in systems operating under high pressure or overloaded conditions.

Information provided by Quaker

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D287
pH 9.5ASTM D70
Viscosity Measurement 220Index; ASTM D2270
Viscosity Measure 43 cSt
@Temperature 40.0 °C
ASTM D445
Storage Temperature 0.000 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Pour Point -34.0 °CASTM D97
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 40 %
 
Descriptive Properties
AppearanceRed, Clear Liquid
Pump Test<50 mg wearASTM D2282
Reserve Alkalinity150-180

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PA6/6 FR 346 RD
Evonik POLYTREND® 850-0940 Colorant
Wacker Pulpsil® 355 Silicone Antifoam Compound
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel

WQUAK006 / 184992

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.