Polyamide 66 with glass fibers and PTFE, heat stabilized, black Main features: Improved friction and wear behavior. Optimized for dry running operations. Heat stabilized. High dimensionally stable precision parts with low warpage and narrow tolerance range. Information provided by Lehmann & Voss & Co.KG |