Pro-fax EP714K impact polypropylene copolymer is available in pellet form. This resin is typically used in thermoforming and sheet extrusion applications and offers excellent stiffness and good antistatic properties. Availability: North America Application: Thermoformed Food Containers Market: Rigid Packaging Processing Method: Sheet; Thermoforming Attribute: Contains Antistat; Good Stiffness; High Heat Resistance; Nucleated Information provided by LyondellBasell. |