MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch-Weld™ EZ250060 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as well as select plastics. This product offers a wide variation of open and set times as well as the ability to produce very thin bond lines. Medium setting, low viscosity ideal for wood and select plastics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Brookfield Viscosity 7000 cP7000 cPThermosel using spindle #27
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
Tensile Strength at Break 29.0 MPa4210 psiASTM D638 Die C
Elongation at Break 675 %675 %ASTM D638 Die C
Shear Strength  2.62 MPa
@Temperature 82.0 °C
380 psi
@Temperature 180 °F
Overlap, Maple
 13.2 MPa
@Temperature 23.0 °C
1910 psi
@Temperature 73.4 °F
Overlap, Maple
 8.34 MPa
@Time Error in fixSigDigits: @digits must be between 1 a sec
1210 psi
@Time Error in fixSigDigits: @digits must be between 1 a hour
Overlap, Maple conditioned for 7 days AT RT/50% RH
 11.89 MPa
@Time 3600 sec
1725 psi
@Time 1.00 hour
Overlap, Maple conditioned for 7 days AT RT/50% RH
 12.6 MPa
@Time 259000 sec
1830 psi
@Time 72.0 hour
Overlap, Maple conditioned for 7 days AT RT/50% RH
 12.72 MPa
@Time 86400 sec
1845 psi
@Time 24.0 hour
Overlap, Maple conditioned for 7 days AT RT/50% RH
 13.2 MPa
@Time 605000 sec
1910 psi
@Time 168 hour
Overlap, Maple conditioned for 7 days AT RT/50% RH
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 min0.0167 hourSet Time
 
Descriptive Properties
Appearancewhite/off-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34753 / 169500

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.