MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TSRC Taipol® 015H BR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polymerization System: Solution Polymerization

Catalyst: Ziegler Cobalt Type

Configuration: 94% cis minimum

Stabilizer: Non-staining

Characteristics: Short dissolving time; Low solution viscosity; Very low gel content; Excellent gloss; Excellent low temperature properties

Application: Mainly for high impact polystyrene (HIPS) modification.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/cc
Volatiles <= 0.50 %<= 0.50 %Polymer Properties; ASTM D-5668
Viscosity 45 - 75 cP45 - 75 cP5% Styrene Solution; ASTM D-3616
Mooney Viscosity 37 - 47
@Temperature 100 °C
37 - 47
@Temperature 212 °F
ML1+4; ASTM D-1646
Ash <= 0.20 %<= 0.20 %Polymer Properties; ASTM D-5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content <= 0.015 %<= 0.015 %insoluble; K62-BRFP-06
 
Descriptive Properties
Color<15APHA, ASTM D-1209
Stabilizer0.7 phrK62-BRFP-23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC016 / 306304

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.