HyTemp NPC-25 is a 25%active dispersion of a proprietary quaternary ammoniumsalt in an acrylic elastomer binder. This 25% active dispersion exhibits fast incorporation during the mixing process. This product provides extremely fast cure, excellent shelf stability and scorch safety to 100°C. The dispersion is in the form of dark blue pellets dusted with clay and free from foreign material. Non-post cure agent used with HyTemp 4050 and 4060 series. (25% active) |