MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Syensqo (Solvay Specialty Polymers) RHODAFAC® ASI 30 Surfactant
Categories: Fluid

Material Notes: Typical Properties: A colorless flowable gel, retaining pourable characteristics down to 0°C. pH 2.3 (5% aqueous dispersion) Miscible with solvents such as industrial denatured alcohol and acetone

Identification: SOLUTION OF OCTYL PHOSPHONIC ACID IN WATER

CAS No : 4724 – 48 – 5

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 28 - 32 %28 - 32 %OPTI067
 
Chemical PropertiesMetricEnglishComments
Acid Value 155 - 185155 - 185[mg KOH/g]; OPTI065
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceColorless flowable gel
Color<50Hazen, OSTM030
Content96%Assay, OPTI066

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shinil Chemical SHINNANO PP Polymer Nanocomposite IP
Noble Polymers Forte™ 4CPP093 Nanocomposite
Chemours Teflon® PTFE Grade K-20 Aqueous Dispersion

PSOLVAY766 / 218494

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.