MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Film Properties. Features: Low gel, good clarity, easy processability.

Applications: Bread bags, HDPE bottle sleeves, specialty blending.

Data provided by the manufacturer.

Key Words: Linear Low Density Polyethylene; Polybutene; Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D792
Moisture Vapor Transmission 0.350 cc-mm/m²-24hr-atmASTM D1434
Water Vapor Transmission 14.0 g/m²/dayASTM D1434
Oxygen Transmission 120 cc-mm/m²-24hr-atmor 4800 cc/m²-atm-24 hr per 25 µm film; 38°C; 90% RH Difference
Melt Flow 1.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 16.0 MPaASTM D882
Film Tensile Strength at Yield, TD 12.0 MPaASTM D882
Film Elongation at Break, MD 600 %ASTM D882
Film Elongation at Break, TD 900 %ASTM D882
Secant Modulus, MD 0.200 GPaASTM D882
Secant Modulus, TD 0.260 GPaASTM D882
Coefficient of Friction 0.20ASTM D1894
Elmendorf Tear Strength, MD 4.00 g/micronASTM D1922
Elmendorf Tear Strength, TD 18.0 g/micronASTM D1922
Dart Drop 2.00 g/micronF 50; ASTM D1709/A
Film Tensile Strength at Break, MD 42.0 MPaASTM D882
Film Tensile Strength at Break, TD 32.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 96.0 °CASTM D1525
Brittleness Temperature <= -68.0 °CASTM D696
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %
@Thickness 0.0250 mm
ASTM D1003
Gloss 57 %45°; 1 mil; ASTM D1894
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 230 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin
LyondellBasell Purell 2410T Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Chevron Phillips Marlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film

PEHN0G / 35529

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.