MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tipco Tipcolene® SEB 300 M - 30% Chemically Coupled Glass Fibers & Mineral Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: 30% Mineral + Glass Reinforced, PP Homopolymer for Automobile Engine Parts

Applications: Automotive Engine Parts

Processing: Injection Molding

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D955
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.0 MPa7400 psiASTM D638
Elongation at Break >= 8.0 %>= 8.0 %ASTM D638
Flexural Yield Strength 68.0 MPa9860 psiASTM D790
Flexural Modulus 3.50 GPa508 ksiASTM D790
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Thermylene® P6-30FG-0709 30% Fiber Glass Reinforced, Heat Stabilized Polypropylene
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper Polypropylene
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene
Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized Polypropylene
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced Polypropylene

PTIP590 / 70324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.