MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco RPM® Arctic Gear Lubricant
Categories: Fluid; Lubricant

Material Notes: Features

Chevron RPM Arctic Gear Lubricant is a multipurpose, heavy duty automotive gear lubricant designed to meet the severe demands of cold weather operations. It is formulated with ISOSYN® base stocks and compounded with extreme pressure, antiwear, corrosion inhibition, rust preventive, and foam suppressant additives, as well as a shear stable viscosity index improver. This additive package is a new generation sulfur-phosphorus system with improved thermal stability, gear spalling protection, and antiwear performance.

Chevron RPM Arctic Gear Lubricant is designed to provide maximum wear protection for automotive gear sets operating in extremely cold conditions, where fluidity of the lubricant is critical to protect gears and bearings. Low viscosity hastens the release of entrained air in the lubricant at low temperatures, thereby providing a better oil film on moving parts.

Applications

Chevron RPM Arctic Gear Lubricant is recommended for all automotive rear axle and manual transmission gears operating in severe arctic climates, or where the manufacturer recommends a viscosity range lighter than conventional SAE 80W 90 or SAE 85W 140 gear lubricants.

Chevron RPM Arctic Gear Lubricant meets the requirements of API Service Categories GL4, GL-5 and MT-1.

It is engineered to pass the performance requirements of SAE J 2360 (formerly known as MIL PRF-2105E).

Key Words: CPS Number: 250412; MSDS Number: 4726
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 28.6 °
Brookfield Viscosity 120000 cP
@Temperature -40.0 °C
Saybolt Viscosity at 100°F 475 SUS
Saybolt Viscosity at 210°F 87 SUS
Kinematic Viscosity at 40°C (104°F) 94 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 16.8 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Timken Test 50.0 lb
 
Thermal PropertiesOriginal ValueComments
Pour Point -45.0 °CASTM D97
 
Descriptive Properties
Channel Point °C-50
Corrosion, Copper Strip Test 3h1B at 120°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV215 / 74830

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.