MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hogen H50S, 50 Silver/50 Tungsten PM Metal Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy; Refractory Metal; Tungsten Alloy

Material Notes: Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.

Silver-Tungsten is used when high oxidation-resistant materials are necessary and superior surface is required. Silver-tungsten is also widely used for tips on contact shoe facings used in high frequency continuous welding processes.

Data provided by Hogen Industries.

Key Words: Hogen Industries Powder Metallurgy Metal Composite; Tungsten Alloys, Silver Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 13.2 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 70
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 50 %
Tungsten, W 50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cadi 50WS Tungsten Silver
Mi-Tech Metals SW50 50 Silver/50 Tungsten PM Metal Composite
CMW® ELKONIUM 46 Silver Alloy
Hogen H20S, 26 Silver/74 Tungsten PM Metal Composite
Hogen H35S, 35 Silver/65 Tungsten PM Metal Composite

NHOG00 / 17308

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.