MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.

Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.

Advantages: Excellent stress crack resistance, high modulus at equal density, excellent dimension stability, better low temperature impact strength, broad molding latitude.

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Base Resin Density 0.938 g/cc0.0339 lb/in³ASTM D1505
ESCR 100% Igepal® >= 1000 hour
@Thickness 3.18 mm
>= 1000 hour
@Thickness 0.125 in
bent strip, non slit; ASTM D1693
Base Resin Melt Index 4.0 g/10 min4.0 g/10 minI2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.7 MPa2570 psiASTM D638
Elongation at Break >= 660 %>= 660 %ASTM D638
Flexural Modulus 0.892 GPa129 ksiASTM D790
1% Secant Modulus 568.78 MPa82495 psiASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 117 °C243 °Fresin; ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene PM96750
LyondellBasell Petrothene GA652962 High Density Polyethylene (HDPE), Rotational Molding Grade
LyondellBasell Microthene MP652962 HDPE
ExxonMobil LLP8460.29 Rotational Molding Resin
Braskem RC35U4 LLDPE Rotomolding Polyethylene

PTITAN48 / 70414

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.