MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2030701P1 Silver/Silver Chloride Paste
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating; Polymer; Thermoset

Material Notes: Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. This is the most common ratio Material used for reference electrodes in medical diagnostics, environmental sensor and the ’agri-food’ industries. It contains a crosslinking resin system for printing on substrates with low adhesion surfaces, i.e.: polyimide.
Screen Printing Equipment: semi-automatic, manual
Screen Types: polyester, mesh 156-230tpi
Substrate: Polyester, PVC, Polycarbonate or ceramic.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 82 - 84 %
@Temperature 150 °C
Viscosity 7000 - 9000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Storage Temperature 20.0 °Csealed container
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.0448 ohm
@Thickness 0.0272 mm
Using a 230 mesh stainless steel screen, 13 micron emulsion
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 150 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Coverage cm2/g81Using a 230 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C60531D1 Silver / Silver Chloride Paste

WGELZ9025 / 139338

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.