MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cosmic Plastics 3D36 Long Glass Filled Alkyd Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Alkyd (Polyester), Molded, Mineral Filler

Material Notes: Description: Cosmic 3D36 is a long glass fiber filled, impact resistant and flame retardant alkyd molding compound which is supplied in a flake form. It molds easily in standard compression or transfer equipment and has a shelf life of one year when stored at 100C or below.

Features: 3D36 cures rapidly to give high strength parts with excellent surface, good electrical insulation and dimensional stability.

Applications: Used in circuit breakers, relays, coil bobbins, terminal boards and connectors.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.95 g/cc
Bulk Factor 6.0 - 12
Water Absorption 0.25 %
@Temperature 50.0 °C,
Time 173000 sec
Linear Mold Shrinkage 0.0010 - 0.0040 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3500 - 7000 psi
Flexural Strength 12000 - 14000 psi
Compressive Strength 18000 - 22000 psi
Izod Impact, Notched 3.00 - 6.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.5
@Frequency 1000 Hz
Dry
 5.5
@Frequency 1e+6 Hz
Wet
 5.6
@Frequency 1e+6 Hz
Dry
 6.0
@Frequency 1000 Hz
Wet
Dielectric Strength 350 V/milWet, step by step
 400 V/milDry, step by step
Dielectric Breakdown 40 VWet, step by step
 55 VDry, step by step
Dissipation Factor 0.025
@Frequency 1e+6 Hz
Dry
 0.030
@Frequency 1e+6 Hz
Wet
 0.040
@Frequency 1000 Hz
Dry
 0.050
@Frequency 1000 Hz
Wet
Arc Resistance 140 sec
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 205 °C
Flammability, UL94 V-1
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 130 - 170 °C
 
Descriptive Properties
Dimensional Stability<0.04%
MIL-M-14MAI-60ASTM D5948-96
Molding Pressure500-8000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram RamTough PZ741 Polycarbonate, UV Stabilized
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Lotte Advanced Materials Infino® PCA-NH1015V Flame Retardant
LG Chemical Lupoy 1200-08 Polycarbonate Resin
Kotec Carbotex KV-75FD Polycarbonate, Food Grade

PCOSM023 / 190805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.