MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass
Categories: Ceramic; Glass

Material Notes: Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 ºF (620 ºC).

Key Words: Coatings
Vendors: Aremco offers a wide range of ceramic, glass and silicone based coatings for ceramic, glass and quartz materials used in heater and lighting applications to 2000°F (1093°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/cc
Solids Content 41.6 %by Volume
 54 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
Viscosity 1000 - 2000 cP
Thickness 1.00 milDry Film Thickness
 2.40 milWet Film Thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1150 °FContinuous
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Cure Time 0.500 - 1.00 hourAir Set prior to curing
 0.500 hour
@Temperature 621 °C
Shelf Life 6.00 Month
 
Descriptive Properties
ColorLight Gray
Theoretical Dry Film Coverage, ft2/gal668@ 1 mil
ThinnerWater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAREM391 / 138319

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.