MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Redwood Plastics Redco™ PTFE VIRGIN
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Redco™ PTFE (Polytrifluoroethylene) offers outstanding properties making it the ultimate choice due a multitude of applications. Redco PTFE has the lowest coefficient of friction, no water absorption, is self lubricating, has excellent chemical resistance and a high temperature tolerance (+500F). Redco™ PTFE is very non-reactive, and so is often used in containers and pipework for reactive chemicals. Its extremely high bulk resistivity also makes it an ideal material for fabricating long life electrets, useful devices that are the electrostatic analogues of magnets. As well, because of its extremely low coefficient of friction, it is used for applications where sliding action of parts is needed: bearings, bushings, gears, slide plates, etc. In these applications it performs significantly better than nylon and acetal; it is comparable with ultra high molecular weight polyethylene (UHMWPE), although UHMWPE is more resistant to wear than PTFE. For these applications, versions of PTFE with mineral oil or molybdenum disulfide embedded as additional lubricants in its matrix are being manufactured.

Applications: Solid pipe and fittings, steel pipe liner and fittings, valve components, expansion bellows, shaft packing and tubing, seals, piston rings, bushings, bearings, wire and cable Insulation, fiber optics coating.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.10 - 2.20 g/cc0.0759 - 0.0795 lb/in³ASTM D792
Water Absorption 0.00 %0.00 %ASTM D570
Deformation 8.0 %8.0 %PERMANENT; ASTM D621
 12 %
@Time 7200 sec,
Pressure 11.1 MPa
12 %
@Time 2.00 hour,
Pressure 1610 psi
23°C; ASTM D621
 15 %
@Time 86400 sec,
Pressure 11.1 MPa
15 %
@Time 24.0 hour,
Pressure 1610 psi
23°C; ASTM D621
 55 %
@Time 7200 sec,
Pressure 11.1 MPa
55 %
@Time 2.00 hour,
Pressure 1610 psi
150°C; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 6560 - 65ASTM D2240
Tensile Strength 15.8 - 34.3 MPa2290 - 4980 psiASTM D638
Elongation at Break 250 - 400 %250 - 400 %ASTM D638
Flexural Strength 5.59 MPa811 psiASTM D790
Flexural Modulus 0.343 - 0.618 GPa49.8 - 89.6 ksiASTM D790
Compressive Strength 3.92 - 4.90 MPa569 - 711 psiASTM D695
Compressive Modulus 0.392 GPa56.9 ksiASTM D695
Impact  9.0
@Temperature -200 °C
9.0
@Temperature -328 °F
[cmkgf/cm2]; ASTM D-256
 15
@Temperature 200 °C
15
@Temperature 392 °F
[cmkgf/cm2]; ASTM D-256
Coefficient of Friction, Dynamic 0.040 - 0.0600.040 - 0.060P-7, V-0.5 m/s
Coefficient of Friction, Static 0.050 - 0.0800.050 - 0.080P-35
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D258
Dielectric Strength 24.0 kV/mm610 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  125 µm/m-°C
@Temperature 30.0 - 150 °C
69.4 µin/in-°F
@Temperature 86.0 - 302 °F
ASTM D-696
 141 µm/m-°C
@Temperature 30.0 - 200 °C
78.3 µin/in-°F
@Temperature 86.0 - 392 °F
ASTM D-696
 155 µm/m-°C
@Temperature 30.0 - 250 °C
86.1 µin/in-°F
@Temperature 86.0 - 482 °F
ASTM D-696
CTE, linear, Transverse to Flow  125 µm/m-°C
@Temperature 30.0 - 150 °C
69.4 µin/in-°F
@Temperature 86.0 - 302 °F
ASTM D-696
 135 µm/m-°C
@Temperature 30.0 - 200 °C
75.0 µin/in-°F
@Temperature 86.0 - 392 °F
ASTM D-696
 164 µm/m-°C
@Temperature 30.0 - 250 °C
91.1 µin/in-°F
@Temperature 86.0 - 482 °F
ASTM D-696
Thermal Conductivity 0.251 W/m-K1.74 BTU-in/hr-ft²-°F
 
Descriptive Properties
Heat Resistance-250 - 260°Cat Atm. Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW044 / 296610

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.