MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik POLYVEST® MA 75 Polybutadienes
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Liquid Polybutadienes: With its POLYVESTR Evonik offers a range of stereospecific, low viscous and unsaponifiable liquid polybutadienes of different chemical composition:
  • POLYVEST®
  • POLYVEST® MA
  • POLYVEST® HT
Our non-functionalized products differ in molar mass and viscosity. The MA-functionalized products are adducts of linear polybutadiene and maleic anhydride and differ in maleic anhydride content and viscosity. The anhydride groups are randomly distributed along the polymer chains and thus make the originally apolar polybutadiene more polar and accessible for various chemical reactions. The hydroxyl-terminated product is an alpha-omega-terminated diol of polybutadiene manufactured by radical polymerisation process. In addition to the double bonds in the polymer backbone, the hydroxyl functional groups provide opportunities for precise chemical modifications. The non-functionalized POLYVESTR grades are supplied in steel drums with 190kgs net. The maleic anhydride-functionalized grades are supplied in steel drums with 180kgs net and 900kgs net IBC. POLYVEST HTR is available in steel drums and IBC. Road tanker delivery is possible for all grades.

Your benefits: The microstructure of our POLYVESTR grades makes them a highly reactive and cross-linking binder and provides them with properties including:

  • excellent chemical resistance
  • high water resistance
  • very good electrical insulation
  • very good cold-resistance
  • low moisture and oxygen permeability
Our POLYVESTR grades can be used in a broad field of applications.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³DIN ISO 2811-1
Viscosity 6000 - 9000 cP
@Temperature 20.0 °C
6000 - 9000 cP
@Temperature 68.0 °F
DIN EN ISO 3219
Molecular Weight 3000 g/mol3000 g/molDIN 55627-1
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 70 - 9070 - 90[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesMetricEnglishComments
Pour Point -25.0 °C-13.0 °FDIN ISO 3016
Glass Transition Temp, Tg -95.0 °C-139 °FDIN EN ISO 11357-1
Flash Point 300 °C572 °FDIN EN ISO 2719
Ignition Temperature 360 °C680 °FDIN 51794
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 2.5<= 2.5DIN EN ISO 4630-2
 
Descriptive Properties
Appearanceviscous liquid
Iodine No.380-420 g Iod/100gDIN 53241

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik POLYVEST® MA 75 Liquid

PEVONIL132 / 196336

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.