MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hexcel® HexWeb® HFT – 1/8 – 4.0 Fiberglass/Phenolic Honeycomb
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Phenolic

Material Notes: Description: HexWeb® HFT® is a fiberglass ± 45 degree Fibertruss® bias weave reinforced/phenolic honeycomb. This bias weave construction enhances the shear modulus properties of the honeycomb core. The shear modulus for HexWeb® Fibertruss® HFT® is about twice that of HRP® (honeycomb made of straight weave fiberglass) and three times that of HRH®-10 (honeycomb made from NOMEX®). This makes HexWeb® Fibertruss® HFT® honeycomb ideal for applications where minimum deflections are required. There is little change in flatwise compression properties due to the bias of the glass. HexWeb® Fibertruss® HFT® has improved damage resistance and handling since the 45 degree angle of the fiber at the cell wall corners allows greater flexibility. This increased flexibility allows the HexWeb® Fibertruss® HFT® to be formed more easily than straight weave honeycombs, resulting in reduced shop losses and simplified fit up of parts during assembly. HexWeb® Fibertruss® HFT® has improved node bond strength and flexibility that makes it possible to offer a 1/8-inch cell fiberglass reinforced honeycomb. This, together with the higher shear properties, makes HexWeb® Fibertruss® HFT® an excellent core for use with high modulus graphite or other composite facing materials. The potential problem of galvanic corrosion with untreated aluminum honeycomb is eliminated, and the small cell size provides uniform support and bonding area for such facings.

Key Features:

  • High shear properties, due to the ±45 degree fiber orientation
  • Small cell size, 1/8 inch minimum hexagonal
  • Improved flexibility; damage resistance, and handling characteristics over conventional 0/90 degree fiber construction
  • High strength retention at temperatures up to 350°F
  • Low moisture pickup
  • Low smoke emission
Applications: HexWeb® Fibertruss® HFT® is ideally suited for use in structural panels where superior nonmetallic core shear properties and/or minimum deflections are required. Typical applications are airfoil, control surfaces, fairings, engine nacelles, bulkheads, helicopter rotor blades, and equipment trays for motion-sensitive block boxes. HexWeb® Fibertruss® HFT® has also been designed into radomes because of its small cell size, dielectric transparency, and ease of handling.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0641 g/cc0.00232 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 2.90 MPa>= 420 psiStabilized; AMS-STD-401
 3.86 MPa560 psiStabilized; AMS-STD-401
Compressive Modulus 0.317 GPa46.0 ksiStabilized; AMS-STD-401
Shear Modulus 0.0827 GPa12.0 ksiW Direction; AMS-STD-401
 0.172 GPa25.0 ksiL Direction; AMS-STD-401
Shear Strength >= 0.827 MPa>= 120 psiW Direction; AMS-STD-401
 1.03 MPa150 psiW Direction; AMS-STD-401
 >= 1.65 MPa>= 240 psiL Direction; AMS-STD-401
 2.17 MPa315 psiL Direction; AMS-STD-401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9245 / 322401

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.