MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite SUMILITE® ELC-4765/EI-6765 Glass Epoxy Laminate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Glass Epoxy Multi-layer Materials for PCB

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.10 %0.10 %E-24/50+D-24/23
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 15.0 GPa2180 ksiTD
 16.0 GPa2320 ksiMD
Flexural Strength 460 MPa66700 psiTD
 620 MPa89900 psiMD
Flexural Modulus 15.0 GPa2180 ksiTD
 16.0 GPa2320 ksiMD
Peel Strength 1.30 kN/m7.42 pli18umCF; S-20"/260
 1.40 kN/m7.99 pli18umCF; A
Film Tensile Strength at Break, MD 260 MPa37700 psi
Film Tensile Strength at Break, TD 250 MPa36300 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmC-96/40/90
 5.00e+15 ohm-cm5.00e+15 ohm-cmA
Surface Resistance 2.00e+14 ohm2.00e+14 ohmC-96/40/90
 1.00e+15 ohm1.00e+15 ohmA
Dielectric Constant  4.5
@Frequency 1e+9 Hz
4.5
@Frequency 1e+9 Hz
 4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
Dissipation Factor  0.014
@Frequency 1e+9 Hz
0.014
@Frequency 1e+9 Hz
 0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 117 µm/m-°C65.0 µin/in-°F10°C/min; Z (a1)
 486 µm/m-°C270 µin/in-°F10°C/min; Z (a2)
CTE, linear, Transverse to Flow 25.2 µm/m-°C14.0 µin/in-°F10°C/min; X (a1)
 28.8 µm/m-°C16.0 µin/in-°F10°C/min; Y (a1)
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FLaser Flash
Glass Transition Temp, Tg 135 °C275 °F10°C/min; TMA
 145 °C293 °F10°C/min; DSC
 150 °C302 °F10°C/min; DMA
Flammability, UL94 V-0V-0Flame Resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Sumitomo Bakelite SUMILITE® ELC-4762 Glass Epoxy
Sumitomo Bakelite SUMILITE® ELC-4768/EI-6768 Glass Epoxy Laminate

PSUMIT107 / 193912

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.