MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Pyro-Bloc C
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyro-Bloc Veneering modules, R Grade, ZR Grade, C Grade are made Pyro-Log fiber turned edge-grain and slightly compressed with a gauze type wrap. Pyro-Bloc Veneering Modules are part of the Unisystem family of products. They can be applied over a variety of refractory surfaces using K-Bond mortar. Unikote M or S surface coatings are normally applied over the module hot face to provide thermal stability and chemical attack resistance.

Features:

  • 12" x 12" (305 mm x 305 mm) blocks of ceramic fiber insulation
  • Easily installed over existing refractory surface
  • Improves furnace efficiency without replacing a serviceable refractory lining
  • Monolithic, edge-grained ceramic fiber modules
  • Maximum temperature rating 2600°F (1427°C)
  • Applications:

  • Forge furnaces
  • Crucible furnace
  • Rotary hearth furnace
  • Holding furnace
  • Heat treating furnace
  • Pusher reheat furnace
  • Ceramic kiln
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.192 g/cc0.00694 lb/in³
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0720 W/m-K
    @Temperature 260 °C
    0.500 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    12 pcf; ASTM C201
     0.138 W/m-K
    @Temperature 538 °C
    0.960 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    12 pcf; ASTM C201
     0.239 W/m-K
    @Temperature 816 °C
    1.66 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    12 pcf; ASTM C201
     0.353 W/m-K
    @Temperature 1090 °C
    2.45 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    12 pcf; ASTM C201
    Maximum Service Temperature, Air 1370 °C2500 °FRating
     1430 °C2600 °FContinuous
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 43 %43 %
    Cr2O3 3.0 %3.0 %
    SiO2 54 %54 %
     
    Descriptive Properties
    Loss on Ignition trace
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM086 / 2406

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.