MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® MDF606 Nylon 6, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Notes: MDF606 is a 30% glass fiber reinforced, impact modified nylon 6 that offers good rigidity and toughness over a wide temperature range. The grade is also stabilized for good weathering performance in outdoor applications.

Availability: Europe; North America

Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Impact Modifier

Features: Good Thermal Stability; Good Toughness; Impact Modified; Medium Rigidity; Weather Resistant

Uses: Outdoor Applications

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.8 %1.8 %50% RH; ISO 62
Linear Mold Shrinkage 0.0070 - 0.014 cm/cm0.0070 - 0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527-2
Elongation at Break 6.0 %6.0 %ISO 527-2
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 6.70 GPa972 ksiISO 178
Izod Impact, Notched (ISO) 14.1 kJ/m²6.70 ft-lb/in²ISO 180
Charpy Impact, Notched 1.81 J/cm²8.60 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 200 °C>= 392 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) >= 190 °C>= 374 °FUnannealed; ISO 72-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Oxygen Index 22 %22 %ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 280 °C482 - 536 °F
Middle Barrel Temperature 250 - 280 °C482 - 536 °F
Front Barrel Temperature 250 - 280 °C482 - 536 °F
Melt Temperature <= 300 °C<= 572 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0598 / 237089

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.