MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC ASAHIKLIN AK-225G Hydrochlorofluorocarbon Solvent
Categories: Fluid; Solvent

Material Notes: AK-225G is an environmentally sensible HCFC. It is thermally stable, nonflammable and recoverable by distillation with no decomposition. It has substantially lower global warming potential (GWP) than PFCs and HFCs and an extremely low ozone depletion potential (ODP). AK-225 is exempt from VOC regulations by the U.S. EPA as described in the Oct. 8, 1996 Federal Register.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/cc
@Temperature 25.0 °C
Liquid
Solubility of Water 0.027 %25°C
Solubility in Water 0.016 %25°C
Viscosity 0.60 cP
@Temperature 25.0 °C
Molecular Weight 202.94 g/mol
Vapor Pressure 0.353 bar
@Temperature 25.0 °C
Surface Tension 16.9 dynes/cm25°C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 35.0 cal/gb.p.
Specific Heat Capacity 1.088 J/g-°C
@Temperature 25.0 °C
Liquid
Melting Point -116 °C
Boiling Point 56.1 °C
 
Descriptive Properties
Global Warming Potential (CO2=1, 100yr ITH)530
KB Value30
Ozone Depletion Potential (CFC-11 = 1.0)0.8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WAGC07 / 74563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.