MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Superior Flux Superior SSF-RMA20 Selective Soldering Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Formulated for Selective Soldering Applications
  • Alcohol Based, RMA-Type Rosin Selective Soldering Flux
  • For use with lead-free and lead-bearing alloys.
  • Higher activity coupled with increased temperature tolerance.
  • Increased activity level to meet flow and melt-points of different Lead-Free solders.
  • Conforms to MIL-F-14256, Type RMA
  • Classified as IPC-STD-004, ROL1
Description: Superior SSF-RMA20 is a Type RMA, mildly activated rosin flux that conforms to MIL-F-14256 (Type RMA), as well as IPC-STD-004, ROL1. This RMA flux contains reduced rosin level so that with proper care, there should not be an issue with clogging of the flux spray or drop jet nozzle. This alcohol based flux promotes the rapid activity necessary for selective soldering, and is also formulated to withstand the higher temperature requirements of selective soldering applications. (Solder temperatures in selective soldering units are often 300 – 340°C, instead of the 245-260°C typically found in wave soldering applications.) Superior SSF-RMA20 leaves a rosin residue that is typically removed with a saponifier, such as Superior Flux’s SyberKleen 2000.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.89 - 7.29 lb/gal
Solids Content 17 %
pH 7.0 - 8.0
 
Thermal PropertiesOriginal ValueComments
Flash Point 53.0 °CTCC Method
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 350 °CSoldering Range
 
Descriptive Properties
Halide Content3.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX133 / 185817

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.