MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dover Chemical KEIL FLO 195 Hydrocarbon Pour Point Depressant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Keil-Flo 195 is a 95% active hydrocarbon pour point depressant. It improves low temperature properties of fluids by inhibiting wax crystal and gel formation. Keil-Flo 195 is ashless, completely resistant to shear, and does not promote corrosion. Keil-Flo 195 exhibits exceptional performance in solvent extracted neutral base stocks, as well as hydrocracked based stocks. Keil-Flo 195 is resistant to both shear and oxidation. Keil-Flo 195 exhibits excellent pour point stability and does not contribute to oil in water emulsion formation, as measured by ASTM D-1401. Keil-Flo 195 may be stored in an original container below 130°F. Wear protective equipment if fighting a fire involving Keil-Flo 195.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/cc
@Temperature 25.0 °C
Density 7.41 lb/gal
Kinematic Viscosity at 100°C (212°F) 995 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -40.0 °F5% in 100 SUS P. Oil
Flash Point >= 205 °CCOC
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 12
 
Descriptive Properties
AppearanceViscous Amber liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER153 / 217772

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.