MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wellman Wellamid® MRGF1475 BK01 20% Mineral/Glass Reinforced Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: Description: Mineral/Glass Reinforced Nylon 66

Information provided by Wellman.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183-87
Filler Content 20 %
Linear Mold Shrinkage, Flow 0.0050 - 0.0090 cm/cmISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cmISO DIS 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 88.0 MPaISO 527-93
Elongation at Break 4.0 %ISO 527-93
Flexural Strength 143 MPaISO 178-93
Flexural Modulus 5.25 GPaISO 178-93
Izod Impact, Notched (ISO) 3.10 kJ/m²ISO 180-93
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned)
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry)
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)

PWEL687 / 72403

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.