MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ovako 55Cr3 SB9257 Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 5000 Series Steel

Material Notes: General Information: 55Cr3 according to Ovako standard is a chromium spring steel with a dash of niobium to be used in quenched and tempered condition; suitable application is for example stabilizer bars.

Information provided by Ovako

Key Words: SB 9257 - 54Cr3, WNr 1.7176, DIN 55Cr3, 527A60, GOST 50ChGA, AISI/SAE/ASTM 5155, 5160
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 330
@Thickness <=30.0 mm
Round bar
Tensile Strength 640 MPa
@Thickness <=30.0 mm
Round bar
Tensile Strength, Yield >= 640 MPa
@Thickness <=30.0 mm
Reh, Round bar
Elongation at Break 17 %
@Thickness <=30.0 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 263 °CMS
 734 °CAC1
 763 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.015 - 0.035 %
Carbon, C 0.53 - 0.56 %
Chromium, Cr 0.70 - 0.80 %
Iron, Fe 98.36 - 98.42 %As Balance
Manganese, Mn >= 0.30 %
Niobium, Nb (Columbium, Cb) 0.025 - 0.035 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.15 %
Sulfur, S <= 0.015 %
Titanium, Ti 0.010 - 0.030 %
 
Descriptive Properties
WeldabilityCEV 0.92max
 Pcm 0.67max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Elmet-Starck ST-100-1 Pure Molybdenum Powder Metallurgy Target
Elmet-Starck Pure Molybdenum Tube Powder Metallurgy Targets

NOVAKO349 / 234648

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.