MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT AS1420-180 1-part, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a heat cured, non-corrosive, neutral cure, 1-part, silicone adhesive sealant. It is one in a range of Addition cure products which are solvent free. It exhibits primerless adhesion to many substrates when cured at temperatures above 100°C. It cures to form a very tough resilient silicone elastomer. This product will not corrode copper or its alloys and is suitable for use with electronic components.

Key Features

  • Fast elevated temperature cure
  • Excellent thermal conductivity
  • Non corrosive
  • Contains 180 micron glass spheres
Application: Electronics, self gapping TIM

Cured Product: after 60 minutes at 120°C

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.06 g/cc0.0744 lb/in³BS ISO 2781
Brookfield Viscosity 43000 cP43000 cPMixed
Linear Mold Shrinkage 0.020 cm/cm0.020 in/in
Storage Temperature <= 15.0 °C<= 59.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767ASTM D2240-95
Tensile Strength 3.10 MPa450 psiISO 37
Elongation at Break 70 %70 %ISO 37
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.70e+15 ohm-cm7.70e+15 ohm-cmASTM D-257
Dielectric Constant 6.06.0ASTM D-150
Dielectric Strength 22.5 kV/mm571 kV/inASTM D-149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 187 µm/m-°C104 µin/in-°F
Thermal Conductivity 1.38 W/m-K9.58 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  1.00 - 5.00 min
@Temperature 175 °C
0.0167 - 0.0833 hour
@Temperature 347 °F
 10.0 - 15.0 min
@Temperature 150 °C
0.167 - 0.250 hour
@Temperature 302 °F
 15.0 - 20.0 min
@Temperature 120 °C
0.250 - 0.333 hour
@Temperature 248 °F
 20.0 - 30.0 min
@Temperature 100 °C
0.333 - 0.500 hour
@Temperature 212 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorGrey
Cure typeAddition Heat Cure
RheologyFlowable
Self BondingYes
Volume Coefficient of Thermal Expansion562 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL006 / 314489

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.