MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Vyncolit® G900 Phenolic Novolac
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Vyncolit® G900 is a glass fiber reinforced resol resin based molding material. It has good mechanical properties, combined with superior electrical insulation properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Key Words: PF-(GF+MD)65
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccISO 1183
Apparent Bulk Density 0.790 g/ccISO 60
Water Absorption 0.11 %ISO 62
Linear Mold Shrinkage 0.0023 in/inISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 114 MPaISO 527-1
Elongation at Break 0.88 %ISO 527-1
Tensile Modulus 18.0 GPaISO 527-1
Flexural Strength 185 MPaISO 178
Flexural Modulus 16.0 GPaISO 178
Flexural Strain at Break 1.28 %ISO 178
Compressive Strength 257 MPaISO 604
Charpy Impact Unnotched 13.4 kJ/m²ISO 179-1
Charpy Impact, Notched 3.40 kJ/m²ISO 179-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.82e+15 ohm-cmIEC 60093
Surface Resistance 7.36e+13 ohmIEC 60093
Dielectric Strength 32.0 kV/mmIEC 60243-1
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 5.00 µm/m-°CTMA
CTE, linear, Transverse to Flow 40.0 µm/m-°CTMA
Deflection Temperature at 1.8 MPa (264 psi) 151 °CISO 75 Af
Deflection Temperature at 8.0 MPa 136 °CISO 75 Cf
Shrinkage 0.070 %Post; ISO 2577
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum B390.0-F Die Casting Alloy
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material
Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material
Lotte Advanced Materials Infino® XP-2165MC PPS, 65% GF + MF
Lotte Advanced Materials Infino® XP-2165BM PPS

PSUMIT499 / 194304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.