Product Description: Staybelite™ Ester 10-E Ester of Hydrogenated Rosin is a pale, thermoplastic resin with the excellent resistance to oxidation and discoloration characteristic of ester resins derived from hydrogenated rosin. It is a glycerol ester of rosin that has been stabilized by hydrogenation and has found wide acceptance as a tackifying resin for many adhesive applications, particularly pressure-sensitive, hot melt and emulsion types. In general, it is useful where there is need for a pale, nonoxidizing, color-stable resin. Application/Uses: - Caulks and Sealants
- Contact Adhesives
- Hot Melt Adhesives
- Laminating
- Nonwovens
- Packaging
- Pressure sensitive adhesives
- Solventborne Adhesives
- Tapes and LabelsWax Modification
Key Attributes: - Easily emulsifiable
- Excellent resistance to oxidation
- Light color
- Low odor
- Medium softening point
- Thermoplastic hydrogenated resin
- Wide solubility and compatibility range
Information provided by Eastman |