Description: VESTODUR CL2130 is a 30 % glass fiber reinforced, self-extinguishing compound for injection molding, based on modified polybutylene terephthalate (PBT).Moldings of VESTODUR CL2130 can be crosslinked by high-energy radiation (ß- or ?-radiation) or heat. The influence of the radiation to the mechanical properties is negligible. The short-term heat resistance is increased up to 350°C depending on the conditions. Crosslinked parts of VESTODUR CL2130 can be used in common soldering processes like surge soldering, vapor phase soldering, and IR soldering which are typical in the electronic industry. The incorporated flame retardant is non-migrating and has no corrosive effects on metal inserts or neighboring metal parts. Due to a special additive this PBT compound can be metallized selectively. Information provided by degussa. Evonik Industries is the successor company to Degussa. |