MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Materion Durox® 98 Aluminum Oxide (Al2O3)
Categories: Ceramic

Material Notes: Ideal for addressing challenges in power electronics, semiconductor manufacturing and more.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.83 g/cc
Water Absorption 0.000 %
Grain Size 2.00 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 85.0
Tensile Strength 152 MPa
Modulus of Elasticity 351 GPa
Flexural Strength 379 MPaMOR
Compressive Strength 2413 MPa
Poissons Ratio 0.220
Fracture Toughness 4.00 MPa-m½
Shear Modulus 144 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 9.40
@Frequency 1.00e+10 Hz
 9.50
@Frequency 1.00e+6 Hz
Dielectric Strength 220 V/mil
@Thickness 6.35 mm
Dissipation Factor 0.000100
@Frequency 1.00e+6 Hz
 0.000100
@Frequency 1.00e+10 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.17 µin/in-°F
@Temperature 25.0 - 1000 °C
Specific Heat Capacity 0.837 J/g-°C
Thermal Conductivity 27.0 W/m-K
 
Descriptive Properties
ColorOff White
Gas Impenetrability10e-8 cc/sec He

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMATER996c / 323449

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.