MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Affinity™ PF 1766 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Affinity PF 1766 Polyolefin Plastomer is an ethylene based plastomer, offers excellent processing and performance in extrusion applications targeting for CPP film. Main Characteristics: Pellet form; Excellent processability. Applications: Extrusion applications

Availability: Asia Pacific; North America

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.864 g/ccASTM D792
Melt Flow 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 290 psiCompression Molded, 20 in/min; ASTM D638
Elongation at Break 600 %Compression Molded, 20 in/min; ASTM D638
Tensile Modulus 203 psi100% Secant, Compression Molded, 20 in/min; ASTM D638
1% Secant Modulus 595 psiFlexural, Compression Molded; ASTM D882
2% Secant Modulus 580 psiFlexural, Compression Molded; ASTM D882
Tear Strength 123 pliDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 93.2 °F
Crystallization Temperature 55.4 °FPeak
Glass Transition Temp, Tg -72.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF378 / 311071

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.