MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical O-Xylene
Categories: Fluid

Material Notes: Aromatic liquid similar to DIESEL

Structure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 isomers; o-, m-, and p-, and isolation of different isomers require high degree of fine distillation since their boiling points are similar.

Uses: Plastic, Polyester, Fiber, M-Xylene resin, Polyester, Fiber, Solvent

CAS: 108-38-3, 95-47-6, 106-42-3 and 100-41-4

Information provided by LG Chemical

Key Words: ortho xylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.8802 g/cc0.8802 g/cc
Vapor Pressure 0.00933 - 0.0120 bar7.00 - 9.00 torrVapor Density=3.7
 
Thermal PropertiesMetricEnglishComments
Melting Point -25.19 °C-13.34 °F
Boiling Point 144.4 °C291.9 °F
Flash Point 27.0 - 32.0 °C80.6 - 89.6 °F
Ignition Temperature 464 - 529 °C867 - 984 °FAutoignition
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.50521.5052
 
Descriptive Properties
Color<20 Pt/Co
 <6Acid Wash
ComponentsEthyl Benzene63.5%
 m-Xylene19%
 o-Xylene8%
 p-Xylene8.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A-Glass Fiber, Generic
Lanxess CS 7979 Glass Fiber
Intercontinental Polymers 1128 Bicomponent PBT/PET Fiber Type - 1.8 Denier X 3 Inches
Hexcel® HexTow® IM7 12K Intermediate Modulus Carbon Fiber (12,000 Filaments)
Hexcel® HexTow® IM6 Intermediate Modulus Carbon Fiber (12,000 Filaments)

PLAY775 / 148785

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.