MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wittenburg Cawiton SN970 SEBS
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Cawiton SN970 is a standard (universal) SEBS with a hardness of 70 Shore A. The mechanical properties of this material are relatively good.

Information provided by Wittenburg Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 2781
Melt Flow 10.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10.3 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ISO 868
Tensile Strength 5.50 MPa798 psiFlow direction; ISO 37
 7.30 MPa1060 psiCross Flow direction; ISO 37
Elongation at Break 480 %480 %Flow direction; ISO 37
 642 %642 %Cross Flow direction; ISO 37
100% Modulus 2.50 MPa363 psiCross Flow direction; ISO 37
 3.00 MPa435 psiFlow direction; ISO 37
200% Modulus 2.90 MPa421 psiCross Flow direction; ISO 37
 3.40 MPa493 psiFlow direction; ISO 37
300% Modulus 3.40 MPa493 psiCross Flow direction; ISO 37
 3.80 MPa551 psiFlow direction; ISO 37
Tear Strength, Total 26.9 N6.05 lb (f)Cross Flow direction; ISO 34-2
 31.1 N6.99 lb (f)Flow direction; ISO 34-2
Compression Set 55 %
@Temperature 70.0 °C,
Time 79200 sec
55 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 60.0 °C86.0 - 140 °FHopper
Rear Barrel Temperature 180 - 220 °C356 - 428 °F
Middle Barrel Temperature 190 - 230 °C374 - 446 °F
Front Barrel Temperature 190 - 230 °C374 - 446 °F
Nozzle Temperature 200 - 240 °C392 - 464 °F
Melt Temperature 180 - 240 °C356 - 464 °F
 
Descriptive Properties
ColorOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWITTN015 / 281765

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.