MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories UL 746B. The materials covered by this program have, in many cases, been investigated with respect to retention of certain critical properties (e.g. dielectric, tensile, impact, and the like) as part of a long-time thermal-aging program conducted in accordance with Underwriters Laboratories Inc. Standard for Polymeric Materials-Long Term Property Evaluations, UL 746B.

Information Provided by Menzolit

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccISO 1183
Water Absorption <= 0.50 %ISO 62
Linear Mold Shrinkage 0.0018 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 0.00 %ISO 527-4
Flexural Strength 80.0 MPa
@Temperature 22.0 °C
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 10.0 GPa
@Temperature 22.0 °C
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
Charpy Impact, Notched 2.50 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Strength 10.0 kV/mmIEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°CISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
Thermal Conductivity 0.700 W/m-K
Maximum Service Temperature, Air 165 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-2
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 170 °CISO 11357-2
Oxygen Index >= 34 %ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 155 °CInjection - Compression molding, matched metal die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Menzolit Menzolit® BMC 2400 Unsaturated Polyester UP
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP
Mar-Bal AltraSet MB2000-5 Thermoset Polyester - Flame and Tracking Resistant Grade
Mar-Bal AltraSet MB2000-10 Thermoset Polyester - Flame and Tracking Resistant Grade
Overview of materials for Thermoset Polyester Glass Filled BMC

PMENZ022 / 100756

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.