MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim Butyl Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Butyl Rubber is used in the production of tire inner tubes, diaphragms of shaper-vulcanizers, latex of butyl rubber and numerous other applications.

Application: BK-1675N is a product of isobutylene and isoprene copolymerization in methyl chloride medium. This type of rubber is used for production of tire inner tubes, diaphragms of shaper-vulcanizers, latex and butyl rubber.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 46 - 56
@Temperature 125 °C
46 - 56
@Temperature 257 °F
ML 1+8
Ash <= 0.40 %<= 0.40 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 19.0 MPa>= 2760 psi
Elongation at Break >= 600 %>= 600 %Ultimate
Tensile Modulus >= 0.00700 GPa
@Strain 400 %
>= 1.02 ksi
@Strain 400 %
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe <= 0.020 %<= 0.020 %
 
Descriptive Properties
Content<1.2%Antiglomerate mass
 0.05-0.2%Stabilizer, Agidol-2 or Acidol 2A
 0.05-0.2%Stabilizer, Irganox 1010
 0.05-0.2%Stabilizer, Wingstey L
 0.05-0.2%Stabilizer, A mix of Agidol2 and Iraganox 1010
Mass losses at drying<0.3%
Viscosity Scattering6spread in one lot

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI040 / 317324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.