MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Fomblin® Y LVAC 06/6 Perfluoropolyether
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Fomblin® Y PFPE perfluoropolyether fluids have the following unique features:
- Low vapor pressure
- Chemical inertness
- High thermal stability
- Good lubricant properties
- No flash or fire point
- Non-toxicity
- Excellent compatibility with metals, plastics, elastomers
- Good aqueous and non-aqueous solvent resistance
- High dielectric properties
- Low surface tension
- Good radiation stability
- Environmentally acceptable

Features: Chemical Resistant; High Density; High Heat Resistance

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.88 g/cc
@Temperature 20.0 °C
0.0679 lb/in³
@Temperature 68.0 °F
ASTM D4052
Viscosity Measurement 7171Viscosity Index; ASTM D2270
Kinematic Viscosity 64 cSt
@Temperature 20.0 °C
64 cSt
@Temperature 68.0 °F
ASTM D445
Molecular Weight 1800 g/mol1800 g/molAverage
Vapor Pressure  1.07e-9 bar
@Temperature 25.0 °C
8.00e-7 torr
@Temperature 77.0 °F
 0.00000400 bar
@Temperature 100 °C
0.00300 torr
@Temperature 212 °F
Evaporation Loss 2.8 %
@Temperature 120 °C
2.8 %
@Temperature 248 °F
Surface Tension 21 dynes/cm
@Temperature 20.0 °C
21 dynes/cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Pour Point -50.0 °C-58.0 °FASTM D97
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4195 / 279995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.