MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Solvay RHODICARE T Surfactant
Categories: Fluid

Material Notes: Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydration rate. It exhibits Pseudo-plastic non-thixotropic behaviour, antisyneresis agent and reduces gel exudation. Approved for Ecocert.

C.T.F.A. /I.N.C.I. Name: XANTHAN GUM

CAS: 11138 - 66 – 2

EINECS: 234 – 394-2

Recommended use level: 0.2 - 1%.

Soluble in water

Compatible with Non-ionic, anionic and amphoteric surfactants.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Sodium salt of an anionic high molecular weight hetero-polysaccharide produced by pure culture fermentation of Xanthomonas campestris, purified by recovery with isopropanol, dried and milled. Thickening and stabilizing hydrocolloid giving aqueous solutions of high viscosity and high yield value even at low concentrations, not affected by temperature. Pseudo-plastic non thixotropic behaviour. Effective suspending and stabilizing agent for multi-phasic systems: aqueous suspensions, emulsions and foams, easily sprayable, flowable, pumpable (creams and lotions, toothpastes…). Thickening agent for creams, suspensions, shampoos, gels; synergistic effect with galactomannanes, glucomannanes. Anti-syneresis agent, reduces gel exudation.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 - 0.800 g/cc0.0253 - 0.0289 lb/in³
Particle Size 180 µm180 µm95 min, 80 mesh; TI-2087
 250 µm250 µm99.5 min, 60 mesh; TI-2087
pH 6.0 - 8.06.0 - 8.01% aqueous sol.; TI-2076
Brookfield Viscosity 1400 - 1700 cP1400 - 1700 cP1% in 1% KCl, LVT, 60 rpm, spindle 3; TI-1110
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceFine powder
ColorCreamy white
Composition2-Propanol<750 ppm, TI-2105
 Arsenic as As<2 ppm, USP
 Ash6.5-16%, TI-0130
 Entero-bacteria & other Gram Neg.Absence in 1g, TI-2185
 Heavy metal as Pb<10 ppm, TI-2109
 Pseudomonas aeruginosaAbsence in 1g, TI-2073
 Staphylococcus aureusAbsence in 1g, TI-2073
 Total viable aerobic count<500 cfu/g, TI-2070
 Yeasts and molds<100 cfu/g, TI-2071
Loss on drying7-13%TI-0515

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD312 / 137543

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.