MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Dyneon™ THV 500A Fluorothermoplastic  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: THV 500A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of an agglomerate. As an agglomerate, it can be used for compounding or compression molding, but this form is generally not used for extrusion or injection molding. It provides a low temperature processing, low flammability, thermal stability, and melt processability. IT can be used to prepare molded parts and extrude films, tubes, profiles, and wire coatings. It is useful for applications that require flexibility, low temperature processing, and good chemical resistance.

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.98 g/cc1.98 g/ccASTM D792
Melt Index of Compound 10 g/10 min
@Load 5.00 kg,
Temperature 265 °C
10 g/10 min
@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Flexural Modulus 0.210 GPa30.5 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FASTM D4591
Oxygen Index >= 75 %>= 75 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
FormAgglomerate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ THV 220G Fluorothermoplastic
3M Dyneon™ THV™ 400 Fluorothermoplastic
3M Dyneon™ THV™ 500 Fluorothermoplastic
3M Dyneon™ THV 220A Fluorothermoplastic
3M Dyneon™ THV 221GZ Fluoroplastic Granules

PDYNE025 / 34833

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.