MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vitro Minerals LA 800 Recycled Glass Powder
Categories: Ceramic; Glass

Material Notes: LA Glass powders are functional fillers and extenders produced from clean, post-industrial, glass feedstocks. X-ray diffraction and scanning electron microscopy confirms that the LA Glass calcium aluminosilicate powders are fully amorphous and contain no crystalline silica. The glass chemistry results in relative chemical inertness, making LA Glass resistant to blooming, blistering, or chemical degradation in harsh environments. LA Glass powders enhance a wide range of paints, coatings, plastics, and adhesives. High consistent brightness, tint retention and stain/scrub resistance can be achieved in most paint and coating systems. LA Glass powders have low oil absorption and can be easily dispersed in water- or solvent-based systems. The feedstocks are certified post-industrial and are free from contaminants associated with post-consumer curbside glass. Vitro Minerals’ processing system and true particle size classification provides consistent product quality for 7 grades (LA-300, LA-350, LA-400, LA-500, LA-600, LA-700, LA-800) with finenesses and brightness covering a range of potential applications. Under a microscope, LA Glass powder particles are transparent, angular-shaped particles with similar dimensions in the x, y and z axis.

Information provided by Vitro Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.50 g/ccASTM D153
Bulk Density 35.0 lb/ft³ASTM C110
Brightness 92 - 93 %Y value
Oil Absorption 29 %ASTM D281
Moisture Absorption at Equilibrium <= 0.50 %Free; ASMT C566
Particle Size 6.0 - 7.0 µmd50 median; Laser interferometer
 20 µmd98 top; Laser interferometer
Particle Mesh Size 325 Mesh>99.9%; ASTM C25
pH 10.5AFS 113-87-S
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.5
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 3500 ohmASTM D2448
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51ASTM D801
 
Component Elements PropertiesOriginal ValueComments
Al2O3 14 - 20 %
B2O3 0.00 - 6.0 %
CaO 20 - 25 %
Fe2O3 <= 1.0 %
Loss on Ignition(%) <= 0.50 %
MgO 0.00 - 5.0 %
Na2O or K2O 8.0 - 14 %
SiO2 50 - 55 %
TiO2 <= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CVITRO913 / 209587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.