MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAPE® PEEK-CF45 Polyetheretherketone, Carbon Fiber Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Carbon fiber reinforced UD-tape made from polyetheretherketone. VESTAPE® PEEK-CF45 is an unidirectional fiber-reinforced tape made from PEEK and HT carbon fibers with a fiber volume content of 45% that shows a high chemical resistance, low water absorption and the suitability for high operating temperatures. VESTAPE® PEEK-CF45 is supplied as a band-shaped semi-finished product showing a width of 160 mm and a thickness of 0.25 mm.

Property data for dry samples.

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Filler Content 45 %45 %Volume. Tape property; EN 2559
 53 %53 %Weight Tape property; EN 2559
Moisture Absorption 0.140 %0.140 %Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1750 MPa254000 psiLaminate property. 0°; Sim. to. ISO 527-5
 1750 MPa254000 psiTape property. 0° Orientation; Sim. to. ISO 527-5
Elongation at Break 1.8 %1.8 %Tape property. 0° Orientation; Sim. to. ISO 527-5
Tensile Modulus 7.50 GPa1090 ksiLaminate property. 90° Orientation; ISO 527-5
 100 GPa14500 ksiTape property. 0° Orientation; Sim. to. ISO 527-5
Flexural Strength 70.0 MPa10200 psi90°, Laminate property; ISO 14125
 1350 MPa196000 psi0°, Laminate property; ISO 14125
Flexural Modulus 7.50 GPa1090 ksi90°, Laminate property; ISO 14125
 100 GPa14500 ksi0°. Laminate property; ISO 14125
Compressive Strength 500 MPa72500 psi0°, Laminate property; ISO 14126
Shear Modulus 3.00 GPa435 ksiG12. Laminate property; ISO 14129
Shear Strength 50.0 MPa7250 psiPerpendicular. 12M, 23°C. Laminate property
 70.0 MPa10200 psiInterlaminar; ISO 14130
 
Thermal PropertiesMetricEnglishComments
Melting Point 340 °C644 °FISO 11357-1/-3
Glass Transition Temp, Tg 151 °C304 °FISO 11357-1/-2
 
Descriptive Properties
Fiber ContentHT carbon
Tape Areal Weight381 g/m2
Tape Thickness0.25 mm
Tape Width160 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK878 / 243085

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.