MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

25Cr-10Ni-7.5W-B COBALT BASED SUPERALLOY CASTINGS FOR GAS TURBINE PARTS, NOZZLE VANES
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes:

Creep and rupture data provided by NIMS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  25.0 - 33.0 MPa
@Temperature 875 °C,
Time 3.60e+8 sec
3630 - 4790 psi
@Temperature 1610 °F,
Time 100000 hour
 37.0 - 49.0 MPa
@Temperature 850 °C,
Time 3.60e+8 sec
5370 - 7110 psi
@Temperature 1560 °F,
Time 100000 hour
 56.0 - 63.0 MPa
@Temperature 825 °C,
Time 3.60e+8 sec
8120 - 9140 psi
@Temperature 1520 °F,
Time 100000 hour
 73.0 - 78.0 MPa
@Temperature 800 °C,
Time 3.60e+8 sec
10600 - 11300 psi
@Temperature 1470 °F,
Time 100000 hour
 89.0 - 100 MPa
@Temperature 775 °C,
Time 3.60e+8 sec
12900 - 14500 psi
@Temperature 1430 °F,
Time 100000 hour
 108 - 125 MPa
@Temperature 750 °C,
Time 3.60e+8 sec
15700 - 18100 psi
@Temperature 1380 °F,
Time 100000 hour
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 23 - 27 %23 - 27 %
Iron, Fe 52.5 - 62.5 %52.5 - 62.5 %As Balance
Nickel, Ni 8.0 - 12 %8.0 - 12 %
Tungsten, W 6.5 - 8.5 %6.5 - 8.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
X-40 Cobalt Alloy (UNS R30031)
MetalTek MAR-M-509® Centri-Vac Nickel Cobalt Based Alloy
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched
Cast Stainless Steel HF, ASTM A297
Cast Stainless Steel CPE20N, ASTM A451

NIMS035 / 77552

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.