MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Vinnapas® 8620 E (Scale-up Product) Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 8620 E (Scale-up Product) is a semi flexible dispersible polymer powder based on vinyl acetate, vinyl chloride and ethylene for long open time and excellent tensile adhesion strength after water immersion. The product is in the process of introduction into industrial use (Scale-up Product). Therefore the product data given are subject to change.

Properties: VINNAPAS® 8620 E (Scale-up Product) is a dispersible polymer powder based on a new generation of terpolymer composed of vinyl acetate, vinyl chloride and ethylene. VINNAPAS® 8620 E (Scale-up Product) is a polymeric binder and is ideal for modifying cementitious and gypsum-based drymix mortars, especially tile adhesives. It provides very good workability; cured mortars with VINNAPAS® 8620 E (Scale-up Product) have improved adhesion, flexibility, deformability and abrasion resistance. VINNAPAS® 8620 E (Scale-up Product) contains a fine mineral filler as an antiblocking agent. It is produced without the use of organic solvents, plasticizers and film-forming agents.

Special features: VINNAPAS® 8620 E (Scale-up Product) has no effect on rheological properties and is a polymer powder in the medium Tg range. It is suitable for formulating high-quality, low-emissions flexible tile adhesive that feature excellent tensile adhesion strength, especially after immersion in water and exposure to freeze/thaw cycles.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 - 0.650 g/ccDIN EN ISO 60
Solids Content >= 98 %DIN EN ISO 3251
Particle Size 400 µmmax 4% over; DIN EN ISO 4610
Ash <= 13 %
 
Descriptive Properties
Appearancewhite to light beige powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9620 / 205149

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.