MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKY 115 H3.0 DUS008 Nylon 6, 15% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled; Nylon 6, Glass Filled, Impact Grade; Nylon 6, Heat Stabilized

Material Notes: PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilized

Former Lanxess product line is now with Envalior.

Key Words: ISO 1874-PA 6-HI,GHR,14-060,GF15
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.228 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPaconditioned, 5 mm/min; ISO 527-1,-2
 115 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 4.0 %5 mm/min; ISO 527-1,-2
 12 %conditioned, 5 mm/min; ISO 527-1,-2
Tensile Modulus 2800 MPaconditioned, 1 mm/min; ISO 527-1,-2
 5600 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 95.0 MPaconditioned, 2 mm/min; ISO 178-A
 185 MPa2 mm/min; ISO 178-A
Flexural Modulus 2500 MPaconditioned, 2 mm/min; ISO 178-A
 4900 MPa2 mm/min; ISO 178-A
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
 80.0 kJ/m²
@Temperature 23.0 °C
conditioned; ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °CISO 75-1,-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection molding; ISO 294
Mold Temperature 80.0 °CInjection molding; ISO 294
Dry Time 2.00 - 6.00 hour
@Temperature 80.0 °C
Moisture Content 0.030 - 0.12 %residual; Karl Fischer test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
Envalior Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Celanese Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Envalior Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced

PLANX0506 / 150465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.