MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 3499-3 X 113393 C Liquid Crystal Polymer (LCP) Glass Fiber - LDS Platable  (discontinued **)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15000 psiASTM D 638
Elongation at Break 2.0 %ASTM D 638
Tensile Modulus 1800 ksiASTM D 638
Flexural Strength 21500 psiASTM D 790
Flexural Modulus 1800 ksiASTM D 790
Izod Impact, Notched 2.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 7.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 525 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 450 °FASTM D 648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 630 - 690 °F
Mold Temperature 150 - 250 °F
Drying Temperature 300 °F
@Time 28800 sec
Dew Point -20.0 °F
Injection Pressure 12000 - 18000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 3499-3 X 113393 A Liquid Crystal Polymer (LCP), Glass Fiber - LDS Platable
Celanese VECTRA E845i LDS LCP, 40% Mineral / Glass Reinforced
Celanese VECTRA E840i LDS LCP, 40% Mineral Reinforced
Avient Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products

PQZVA11241 / 120588

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.