MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alfa Chemistry Materials Scandium Fluoride
Categories: Ceramic; Halide

Material Notes: Scandium Fluoride is applied in optical coating, catalyst, electronic ceramics, laser industry, and also the main materials for making Scandium metal and alloys. The main application of Scandium by weight is in Scandium-Aluminum alloys for minor aerospace industry components. Some items of sports equipment, which rely on high performance materials, have been made with Scandium-Aluminum alloys, including baseball bats, and bicycle frames and components. Lacrosse sticks are also made with Scandium. The American firearm manufacturing company Smith & Wesson produces revolvers with frames composed of Scandium alloy and cylinders of Titanium or Carbon steel.

Applications: catalyst, electronic ceramics, laser industry, and also the main materials for making Scandium Metal and alloys.

Solubility: Insoluble in water and strong mineral acids

Molecular Formula: ScF3

Alfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 3.84 g/cc0.139 lb/in³
Solubility in Water 0.00 %0.00 %Insoluble
Molecular Weight 102 g/mol102 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1515 °C2759 °F
 
Descriptive Properties
AppearanceWhite Solid
CAS Number13709-47-2
Purity99.999% 99.99% 99.9%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA66538 / 304823

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.