MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

USI Corporation LINATHENE® LL120 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade; Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Description: LINATHENE ® LL120 is a linear low density polyethylene resin (LLDPE) for use in cast film extrusion and blown film extrusion. This resin is supplied in pellet form and contains an antiblocking agent and a slip agent.

Characteristics:

  • Excellent toughness
  • Great tensile strength
  • Great elongation
  • Outstanding puncture strength
Main Application:
  • Suit Interlining
  • Garment bag
  • Frozen food bags

Information provided by USI Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D792
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.3 MPa1640 psiASTM D882
Film Tensile Strength at Yield, TD 9.81 MPa1420 psiASTM D882
Film Elongation at Break, MD 450 %450 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Film Tensile Strength at Break, MD 24.5 MPa3550 psiASTM D882
Film Tensile Strength at Break, TD 17.7 MPa2570 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FASTM D3418
Vicat Softening Point 103 °C217 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUSIC036 / 285404

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.